LEFM-Based Evaluation of Structural Stress Approaches for Fatigue Assessment of Welded CHS with Large Geometric Scale Differences

Büyük geometrik ölçek farklarına sahip kaynaklı dairesel boru bağlantılarında yorulma değerlendirmesi için yapısal gerilme yaklaşımlarının LEFM tabanlı karşılaştırması

Orijinal makale İngilizcedir; bu özet Türkçeye uyarlanmıştır.

Stefan Vogts, Jörg Baumgartner, Julian Unglaub, Klaus Thiele · Research Square · 2026-11-06 · 7 min read
Five ways of defining the 'structural' (hot-spot) stress at a welded tube-to-shell joint were compared on hundreds of parametric Abaqus models and benchmarked against a fracture-mechanics crack-growth reference. The stress taken 1 mm below the weld toe (Xiao–Yamada) tracked the crack-growth reference almost perfectly, Dong's through-thickness membrane+bending stress came second, and the classic two-point surface extrapolations (IIW, IIW/CIDECT, DNV) scattered the most, especially for joints outside the usual tubular-joint parameter ranges.Kaynaklı bir boru-kabuk bağlantısında 'yapısal' (sıcak nokta) gerilmeyi tanımlamanın beş yolu, yüzlerce parametrik Abaqus modelinde karşılaştırılıp kırılma mekaniğine dayalı bir çatlak büyümesi referansıyla kıyaslandı. Kaynak dibinin 1 mm altından okunan gerilme (Xiao–Yamada) referansı neredeyse birebir izledi, Dong'un kalınlık boyunca membran+eğilme gerilmesi ikinci oldu. Klasik iki noktalı yüzey ekstrapolasyonları (IIW, IIW/CIDECT, DNV) ise özellikle alışılmış boru bağlantısı parametre aralıklarının dışında en fazla saçılmayı gösterdi.

Component & loads
Single-sided welded circular hollow section (CHS) brace on a large monopile-type shell (offshore boat-landing attachment). Five load cases: chord axial, chord in-plane bending, brace axial, brace out-of-plane bending, brace in-plane bending (Table 3).
Software
Abaqus/Standard 2025, models generated automatically through the Abaqus Python interface.
Elements & mesh
Linear hex C3D8R for tubes, linear wedge C3D6 for the weld. Fine/transition/coarse zoning; 8 elements through the chord wall (less than 3% SCF change with further refinement, Fig. 13). A separate submodel with 0.25 mm elements at the weld toe for the 1 mm stress (Fig. 14).
Material model
Linear elastic steel, E = 210 GPa, ν = 0.3.
Boundary conditions
Half model with symmetry, or antisymmetry for brace in-plane bending; chord cut to a half-circumference (less than 1% effect); chord length fixed at α = 2L/d0 = 2. Three boundary-condition sets depending on load symmetry (Fig. 10).
Analysis type
Linear static, parametric Design of Experiments: screening full factorial, then a central composite inscribed design, then response-surface models per load case, evaluation path and stress method.
Assessment method
SCF = structural stress / nominal stress (1 MPa nominal). Methods compared: IIW plate 0.4t/1.0t extrapolation, IIW/CIDECT CHS, DNV-RP-C203 CHS, Xiao–Yamada 1 mm stress, Dong structural stress (stress-based variant, membrane + bending by integration through the thickness).
Standard / criterion
IIW fatigue recommendations, IIW/CIDECT tubular guidance, DNV-RP-C203, AWS D1.1 (weld profile). Reference: analytical LEFM with weight functions, initial crack a = 0.1 mm (a/c = 1), Paris law C = 1.8e-13, m = 3, failure at half the chord wall thickness.
Validation
No physical tests. LEFM is used as an independent computational reference; the authors stress that experimental validation is still needed.
Result & verdict
Correlation of SCF with the LEFM-derived FAT: XY R² = 0.999, Dong 0.980, DNV 0.955, IIW and IIW/CIDECT 0.946. Remaining scatter Tσ (Q90/Q10): XY 1.07, Dong 1.33, DNV 1.51, IIW/CIDECT 1.66, IIW 1.65, versus 8.84 for nominal stress (Fig. 16–17).
Bileşen ve yükler
Büyük monopil tipi bir kabuğa tek taraflı kaynaklı dairesel boru (CHS) bağlantı (açık deniz iskele ataşmanı). Beş yük durumu: kord eksenel, kord düzlem içi eğilme, branş eksenel, branş düzlem dışı eğilme, branş düzlem içi eğilme (Tablo 3).
Yazılım
Abaqus/Standard 2025; modeller Abaqus Python arayüzüyle otomatik üretiliyor.
Elemanlar ve ağ
Borular için doğrusal heksa C3D8R, kaynak için doğrusal kama C3D6. İnce/geçiş/kaba bölgeler; kord cidarında kalınlık boyunca 8 eleman (daha fazla inceltme SCF'yi %3'ten az değiştiriyor, Şekil 13). 1 mm gerilmesi için kaynak dibinde 0,25 mm elemanlı ayrı bir alt model (Şekil 14).
Malzeme modeli
Doğrusal elastik çelik, E = 210 GPa, ν = 0,3.
Sınır koşulları
Simetrili (düzlem içi eğilmede antisimetrili) yarım model; kord yarım çevreye kesilmiş (etkisi %1'den az); kord boyu α = 2L/d0 = 2 sabit. Yük simetrisine göre üç farklı sınır koşulu seti (Şekil 10).
Analiz tipi
Doğrusal statik, parametrik deney tasarımı: tarama amaçlı tam faktöriyel, ardından merkezi kompozit tasarım ve her yük durumu, değerlendirme yolu ve gerilme yöntemi için yanıt yüzeyi modelleri.
Değerlendirme yöntemi
SCF = yapısal gerilme / nominal gerilme (1 MPa nominal). Karşılaştırılan yöntemler: IIW plaka 0,4t/1,0t ekstrapolasyonu, IIW/CIDECT CHS, DNV-RP-C203 CHS, Xiao–Yamada 1 mm gerilmesi, Dong yapısal gerilmesi (gerilme tabanlı türev, kalınlık boyunca integral ile membran + eğilme).
Standart / kriter
IIW yorulma önerileri, IIW/CIDECT boru rehberi, DNV-RP-C203, AWS D1.1 (kaynak profili). Referans: ağırlık fonksiyonlu analitik LEFM, başlangıç çatlağı a = 0,1 mm (a/c = 1), Paris yasası C = 1,8e-13, m = 3, kord cidar kalınlığının yarısında hasar.
Doğrulama
Fiziksel test yok. LEFM bağımsız bir hesaplamalı referans olarak kullanılıyor; yazarlar deneysel doğrulamanın hâlâ gerekli olduğunu vurguluyor.
Sonuç ve hüküm
SCF ile LEFM'den türetilen FAT arasındaki korelasyon: XY R² = 0,999, Dong 0,980, DNV 0,955, IIW ve IIW/CIDECT 0,946. Kalan saçılma Tσ (Q90/Q10): XY 1,07, Dong 1,33, DNV 1,51, IIW/CIDECT 1,66, IIW 1,65; nominal gerilmede 8,84 (Şekil 16–17).

Context

Offshore monopiles often carry welded secondary steel such as boat landings. The welded connection is a small brace on a huge, thick shell: diameter ratios β of about 0.015–0.15 and chord slenderness γ0 up to 130. Most of that range sits outside the parameter windows behind the standard tubular-joint SCF formulas and hot-spot extrapolation rules (Fig. 2). Engineers still routinely apply the usual hot-spot recipe to these joints. The question the paper asks is simple and very practical: when your joint is outside the 'textbook' range, which structural stress definition can you still trust?

Model setup

The joint geometry is fully parametrised (Table 1): brace and chord diameters and thicknesses plus brace inclination up to 25°. A Python script builds every design point in Abaqus, including an explicit solid weld whose fillet size follows the AWS D1.1 flat-profile concept. The fillet size changes continuously with the local dihedral angle around the intersection (Eq. 16). That level of weld detail is unusual in parametric studies and is worth noting if you build solid weld models yourself.

Model reduction is done carefully. A half model uses symmetry or antisymmetry depending on the load case. The authors also check that cutting the chord to half its circumference changes the SCF by less than 1%. The chord length is fixed at twice the chord diameter, and they flag that the results depend on this choice.

Mesh: the hot-spot read-out region uses 8 linear hex elements through the chord thickness, chosen from a convergence study at the two extremes of the thickness ratio τ. The 1 mm stress cannot be read from the global mesh, so they drive a submodel from the global displacements. The submodel boundary sits 3 × t0 away from the weld toe and uses 0.25 mm elements, giving four elements within the first millimetre.

The five stress definitions

  • IIW plate extrapolation: surface stress at 0.4t and 1.0t from the toe, extrapolated linearly; element size normal to the toe no larger than 0.4t.
  • IIW/CIDECT CHS: first point at 0.4t, second point depends on the tube geometry (Table 2).
  • DNV-RP-C203 CHS: both points depend on the geometry (based on √(rt)); a Gauss-point shortcut is also allowed.
  • Xiao–Yamada (XY): normal stress 1 mm below the toe, along the expected crack path. No thickness correction is needed because the subsurface gradient already captures size effects.
  • Dong structural stress: membrane plus bending from integrating the through-thickness normal stress (Eqs. 3–4). The paper notes Dong's method is the basis of the structural-stress fatigue route in the ASME pressure-vessel and fitness-for-service codes. The authors used the stress-based (mesh-sensitive) variant, not the nodal-force variant that ASME relies on for mesh insensitivity.

The clever part: an independent yardstick

There were no fatigue tests, so the authors built a computational reference that does not depend on any of the five definitions. They take the through-thickness stress from the FE model, compute stress intensity factors with weight functions, and grow a 0.1 mm initial crack with the Paris law (IIW constants) until it reaches half the wall thickness. The life is then converted to an equivalent nominal FAT class at 2 million cycles.

If a stress definition captures geometry correctly, multiplying each geometry's LEFM FAT by its SCF should collapse all geometries onto one value. The residual spread is measured as Tσ, the ratio of the 90th to the 10th percentile; 1.0 would be a perfect collapse.

Results

  • The methods are not interchangeable by a constant factor. The ratio to IIW plate extrapolation varies with load case, position and geometry (Fig. 15). DNV is generally higher than IIW plate; IIW/CIDECT stays closest to it. XY gives SCFs about 1.5× higher, with the largest spread under brace in-plane bending at the crown.
  • Collapse quality: nominal stress leaves a scatter of 8.84. All structural-stress methods help a lot, but XY (1.07) and Dong (1.33) clearly beat the surface extrapolations (1.51–1.66) (Fig. 17).
  • Why: with such large scale differences, the geometry-dependent extrapolation points land at very different places on the stress gradient, sometimes close to the toe and sometimes almost in the nominal field. Methods that look into the thickness along the crack path (XY, Dong) see the gradient that actually drives crack growth.
  • Governing parameters: chord loading is driven mainly by the thickness ratio τ and brace slenderness γ1. Brace loading also depends on chord slenderness γ0 and diameter ratio β, with real interaction and quadratic effects, so simple parametric SCF equations do not extrapolate well. Out-of-plane bending loads the saddle, in-plane bending the crown, and axial loading both.
  • The response-surface surrogates fit well at the saddle and less well for axial brace load at the crown (NRMSE about 9%, Table 4). The authors use them for trends only, not as design equations.

How they judged it

There is no pass/fail verdict on a structure. The 'acceptance' question is about methods: which stress definition normalises the geometry effect best? The conclusion is that XY, then Dong, are most consistent with fracture mechanics, and that IIW/DNV tubular extrapolation rules should be checked, not assumed, for joints outside their calibration range. They also point out that each method needs its own S-N curve because the SCF levels differ systematically.

Critique & caveats

  • 'Best agreement with LEFM' is not 'best agreement with tests'. The XY method evaluates stress along the same path the LEFM model uses, so it is naturally favoured. The authors acknowledge this.
  • The weld is idealised (no undercut, misalignment or convexity variation), the chord length is fixed, and the material is linear elastic, which is fine for high-cycle structural stress.
  • They used the mesh-sensitive Dong variant. The nodal-force variant (as in ASME) might do better and would be the one you would actually use under ASME VIII-2.
  • This is a preprint (Research Square) and not yet peer-reviewed. The data set is public on Zenodo (doi:10.5281/zenodo.23345009).

Bağlam

Açık deniz monopilleri genellikle iskele gibi kaynaklı ikincil çelik elemanlar taşır. Kaynaklı bağlantı, büyük ve kalın bir kabuk üzerindeki küçük bir branştır: çap oranı β yaklaşık 0,015–0,15 ve kord narinliği γ0 130'a kadar. Bu aralığın büyük kısmı, standart boru bağlantısı SCF formüllerinin ve sıcak nokta ekstrapolasyon kurallarının dayandığı parametre pencerelerinin dışında kalıyor (Şekil 2). Mühendisler yine de bu bağlantılara rutin olarak alışılmış sıcak nokta yöntemini uyguluyor. Makalenin sorusu basit ve çok pratik: bağlantınız 'ders kitabı' aralığının dışındaysa hangi yapısal gerilme tanımına hâlâ güvenebilirsiniz?

Model kurulumu

Bağlantı geometrisi tamamen parametrik (Tablo 1): branş ve kord çapları ve kalınlıkları ile 25°'ye kadar branş eğimi. Bir Python betiği her tasarım noktasını Abaqus'ta kuruyor; fillet boyutu AWS D1.1 düz profil yaklaşımını izleyen açık bir katı kaynak modeli de dahil. Fillet boyutu, kesişim etrafındaki yerel dihedral açıyla sürekli değişiyor (Denklem 16). Parametrik çalışmalarda bu düzeyde kaynak detayı nadirdir; kendi katı kaynak modellerinizi kuruyorsanız not etmeye değer.

Model indirgeme dikkatle yapılmış. Yük durumuna göre simetrili veya antisimetrili yarım model kullanılıyor. Yazarlar ayrıca kordu yarım çevreye kesmenin SCF'yi %1'den az değiştirdiğini kontrol ediyor. Kord boyu kord çapının iki katında sabit tutulmuş ve sonuçların bu seçime bağlı olduğu belirtilmiş.

Ağ: Sıcak nokta okuma bölgesinde kord kalınlığı boyunca 8 doğrusal heksa eleman var; bu sayı kalınlık oranı τ'nun iki uç değerinde yapılan yakınsama çalışmasıyla seçilmiş. 1 mm gerilmesi global ağdan okunamadığı için global deplasmanlarla sürülen bir alt model kullanılıyor. Alt model sınırı kaynak dibinden 3 × t0 uzakta ve 0,25 mm elemanlarla ilk milimetrede dört eleman sağlanıyor.

Beş gerilme tanımı

  • IIW plaka ekstrapolasyonu: Dipten 0,4t ve 1,0t uzaklıktaki yüzey gerilmesi doğrusal ekstrapole edilir; dibe dik eleman boyu 0,4t'yi geçmemeli.
  • IIW/CIDECT CHS: İlk nokta 0,4t'de, ikinci nokta boru geometrisine bağlı (Tablo 2).
  • DNV-RP-C203 CHS: Her iki nokta da geometriye bağlı (√(rt) esaslı); Gauss noktası kısayoluna da izin var.
  • Xiao–Yamada (XY): Beklenen çatlak yolu boyunca dibin 1 mm altındaki normal gerilme. Yüzey altı gradyan boyut etkilerini zaten yakaladığı için kalınlık düzeltmesi gerekmez.
  • Dong yapısal gerilmesi: Kalınlık boyunca normal gerilmenin integrali ile membran ve eğilme (Denklem 3–4). Makale, Dong yönteminin ASME basınçlı kap ve kullanıma uygunluk kodlarındaki yapısal gerilme yorulma yolunun temeli olduğunu belirtiyor. Yazarlar ASME'nin ağdan bağımsızlık için dayandığı düğüm kuvveti türevini değil, gerilme tabanlı (ağa duyarlı) türevi kullanmış.

Akıllıca kısım: Bağımsız bir ölçüt

Yorulma testi olmadığından yazarlar, beş tanımdan hiçbirine bağlı olmayan hesaplamalı bir referans kurmuş. FE modelinden kalınlık boyunca gerilme alınıyor, ağırlık fonksiyonlarıyla gerilme şiddet faktörleri hesaplanıyor ve 0,1 mm'lik başlangıç çatlağı Paris yasasıyla (IIW sabitleri) cidar kalınlığının yarısına kadar büyütülüyor. Ömür daha sonra 2 milyon çevrimde eşdeğer nominal FAT sınıfına çevriliyor.

Bir gerilme tanımı geometriyi doğru yakalıyorsa, her geometrinin LEFM FAT değerini kendi SCF'siyle çarpmak tüm geometrileri tek bir değerde toplamalıdır. Kalan dağılım Tσ (90. ve 10. yüzdelik oranı) ile ölçülüyor; 1,0 mükemmel toplanma demek.

Sonuçlar

  • Yöntemler sabit bir katsayıyla birbirine çevrilemiyor. IIW plaka ekstrapolasyonuna oran yük durumu, konum ve geometriyle değişiyor (Şekil 15). DNV genelde IIW plakadan yüksek; IIW/CIDECT ona en yakın. XY yaklaşık 1,5 kat daha yüksek SCF veriyor; en büyük yayılım branş düzlem içi eğilmede tepe noktasında.
  • Toplanma kalitesi: Nominal gerilme 8,84'lük bir saçılma bırakıyor. Tüm yapısal gerilme yöntemleri çok yardımcı oluyor, ancak XY (1,07) ve Dong (1,33) yüzey ekstrapolasyonlarını (1,51–1,66) açıkça geçiyor (Şekil 17).
  • Neden: Bu kadar büyük ölçek farklarında geometriye bağlı ekstrapolasyon noktaları gradyan üzerinde çok farklı yerlere düşüyor; bazen dibe çok yakın, bazen neredeyse nominal alanda. Çatlak yolu boyunca kalınlığın içine bakan yöntemler (XY, Dong) çatlak büyümesini gerçekten yönlendiren gradyanı görüyor.
  • Belirleyici parametreler: Kord yüklemesinde başta kalınlık oranı τ ve branş narinliği γ1 etkili. Branş yüklemesinde kord narinliği γ0 ve çap oranı β da devreye giriyor ve gerçek etkileşim ve ikinci derece terimler var; bu yüzden basit parametrik SCF denklemleri iyi ekstrapole edilemiyor. Düzlem dışı eğilme semer bölgesini, düzlem içi eğilme tepe noktasını, eksenel yük ise ikisini birden zorluyor.
  • Yanıt yüzeyi vekil modelleri semer bölgesinde iyi, tepe noktasındaki eksenel branş yükünde daha zayıf uyum gösteriyor (NRMSE yaklaşık %9, Tablo 4). Yazarlar bunları tasarım denklemi olarak değil, yalnızca eğilimler için kullanıyor.

Nasıl değerlendirdiler

Bir yapı için geçti/kaldı hükmü yok. 'Kabul' sorusu yöntemlerle ilgili: geometri etkisini en iyi normalize eden gerilme tanımı hangisi? Sonuç: Kırılma mekaniğiyle en tutarlı olanlar XY ve ardından Dong; IIW/DNV boru ekstrapolasyon kuralları ise kalibrasyon aralığı dışındaki bağlantılarda varsayılmamalı, kontrol edilmeli. Yazarlar ayrıca SCF seviyeleri sistematik olarak farklı olduğu için her yöntemin kendi S-N eğrisine ihtiyaç duyduğunu vurguluyor.

Eleştiri ve çekinceler

  • 'LEFM ile en iyi uyum' 'testlerle en iyi uyum' demek değildir. XY yöntemi gerilmeyi LEFM modelinin kullandığı aynı yol boyunca değerlendirdiğinden doğal olarak avantajlı; yazarlar da bunu kabul ediyor.
  • Kaynak idealize edilmiş (yanma oluğu, eksen kaçıklığı veya bombe değişimi yok), kord boyu sabit ve malzeme doğrusal elastik; yüksek çevrimli yapısal gerilme için bu uygun.
  • Ağa duyarlı Dong türevini kullanmışlar. Düğüm kuvveti türevi (ASME'deki gibi) daha iyi sonuç verebilir ve ASME VIII-2 kapsamında gerçekte kullanacağınız da odur.
  • Bu bir ön baskı (Research Square) ve henüz hakem değerlendirmesinden geçmedi. Veri seti Zenodo'da açık (doi:10.5281/zenodo.23345009).

Vogts, S., Baumgartner, J., Unglaub, J., & Thiele, K. (2026). LEFM-Based Evaluation of Structural Stress Approaches for Fatigue Assessment of Welded CHS with Large Geometric Scale Differences. Research Square (preprint, version 1). https://doi.org/10.21203/rs.3.rs-11376797/v1
· Open-access copy
Original licence: CC BY 4.0